[Introduction]: Xinhai tailings re-processing line, with the thought of protecting ecosystem and fully using resources, provide a re-processing for those valuable metal or non-metal tailings. According different property of all kinds of ore tailings, Xinhai can design reasonable process and fully find the value in the tailings.
[Improvement]: Xinhai tailings re-processing line applies to re-processing of various metal or non-metal tailings, including iron, gold, lead-zinc, copper, fluorite, wolfram, phosphate, graphite, bauxite, etc.
The iron tailings discharge from iron ore plant is in large amount, fine size and different types, and complex property, so Xinhai use the process of magnetic separation, flotation, acid leaching and flocculation to recover iron.
Xinhai usually use all-slime cyanide process and carbon-in-pulp process to recover the gold from gold tailings. As for the gold tailings cyaniding, xinhai will apply the method of dry-tailing stacking. That is, though the process of classifying and dewatering, at the same recycling the water recourses to remove the cyanide in it. Moreover, xinhai will use magnetic separation and gravity separation to remove the iron.
The main component of the lead-zinc tailings are quartz and suicide sericite. Except the methods of stockpiling in tailings pool, dry-tailing stacking and mine filling, Xinhai will also apply gravity separation, flotation separation, magnetic separation, gravity - flotation separation, and other process to recycle the valuable elements.
If the copper with high heavy metals content, the separation will be easier and apply the process of flotation. If there exist magnetite in the copper tailings, it will firstly using acid leaching to precipitate the copper, then use magnetic separation accordingly.
Xinhai use the process of flotation to reselect the fluorite, roughing and then cleaning. Before roughing, the pulp and the reagent will be fully stirred. After that repeated cleaning will be proceed.
Xinhai will apply gravity separation, magnetic separation and flotation separation to recycle the wolfram. The gravity separation is commonly used. Wolfram tailing re-selection process is mainly used spiral chute and centrifugal ore separator to roughing, shaking table and flotation to cleaning.
Siliceous collophanite mainly include quartz siliceous minerals in gangue mineral, so the floatability of gangue is larger than valuable mineral.
Xinhai will use the process of stage grinding and screening to recover the graphite from tailings. In the process of separation, flotation and shaking table is always used. If we want to achieve comprehensive recovery of several kinds of minerals from graphite tailings, we should combine several separation methods.
When deal with the bauxite tailings, flotation separation and magnetic separation is the common process. Moreover, wetting, dry-tailing stacking and mine filling is always used.
To find out more about our products and solutions, please fill out the form below and one of our experts will get back to you shortly.